Spinning SU 8 over AZ9260
2011-08-10
sumit kalsi
2011-08-10
Kevin Nichols
2011-08-11
Jerry Chen
2011-08-12
sumit kalsi
Spinning SU 8 over AZ9260
Jerry Chen
2011-08-11
I also have the same problem, would like to use a sacrificial layer to
release the crosslinked SU8, AZ 40xt was used and not successful.

but did you try the AZ100 resist stripper?

--------------------------------------------------
From: "Kevin Nichols" 
Sent: Wednesday, August 10, 2011 9:56 PM
To: "General MEMS discussion" 
Subject: Re: [mems-talk] Spinning SU 8 over AZ9260

> Use omnicoat from microchem as a release layer.
>
> - Kevin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review