Avoiding photoresist reticulation (burning) during DRIE
2011-09-30
Sarah McQuaide
2011-10-02
Shay
Avoiding photoresist reticulation (burning) during DRIE
Sarah McQuaide
2011-09-30
I sometimes see photoresist reticulation during a device release step using
DRIE, mainly on devices at the edge of the wafer where the release first
happens. Has anyone experimented with ways to avoid resist reticulation
during DRIE? This is a thick resist, challenging to remove later using a
required dry etch.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing