A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to make texturing surface for ZnSe
How to make texturing surface for ZnSe
2011-10-12
weiquan yang
2011-10-12
Ramesham, Rajeshuni (5132)
2011-10-12
Bill Moffat
2011-10-13
weiquan yang
How to make texturing surface for ZnSe
Ramesham, Rajeshuni (5132)
2011-10-12
You can use the diamond paste to roughen the surface.  This is commercially
available.  RIE etching  is OK.  Good luck!  Ram

-----Original Message-----
From: [email protected] [mailto
:[email protected]] On Behalf Of
weiquan yang
Sent: Wednesday, October 12, 2011 9:23 AM
To: [email protected]
Subject: [mems-talk] How to make texturing surface for ZnSe

Hello, everyone

As we know, we can make texturing structure (pyramids) on Si by simple wet
etching. Is there anyone knowing that how to make the texturing surface for
ZnSe? Or some other ways to roughen the surface of ZnSe? The purpose is to
scatter the light and increase the light absorption.What I am thinking about is
using RIE etching or mechanical roughen. I don't know whether is possible or
not.

Regards

Weiquan Yang
Arizona State University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics