MEMSnet Home: MEMS-Talk: cleaning e-beam litography sample
cleaning e-beam litography sample
2011-11-07
Judith Linacero Blanco
2011-11-07
Jack
2011-11-07
Sk Fahad Chowdhury
2011-11-07
G. Puebla-Hellmann
2011-11-08
Jorge Ramiro
2011-11-09
Judith Linacero Blanco
2011-11-10
Judith Linacero Blanco
2011-11-07
Matthieu Nannini, Dr.
2011-11-07
Alexander Slesarev
cleaning e-beam litography sample
Sk Fahad Chowdhury
2011-11-07
If your sample/ process permits, do a O2 plasma cleaning ... 75Watt, 1 min,
20 sccm O2 should clean things up

Fahad

On Mon, Nov 7, 2011 at 8:49 AM, Judith Linacero Blanco
wrote:

> Hello everyone,
>
> I made a lithography by e-beam with lines of 200nm separated 200nm with
> 300nm of PMMA on silicon.
>
> Once I etch the silicon with RIE, and then I try to clean the
> sampleacetone,
> sonicated. The problem is that I still have traces of PMMA in the sample,
> and I can't clean at all the sample.
>
> Can anyone help? How I can clean the whole sample of e-beam lithography?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.