NIL stamp
2011-11-14
Andrea Mazzolari
2011-11-14
righeira carnegie
2011-11-14
Andrea Mazzolari
2011-11-14
GEORGE GREGOIRE
2011-11-14
K.Vossough
NIL stamp
Andrea Mazzolari
2011-11-14
Hi,

min size i need to print is 100nm. I do not know if i need an hard stamp
or a PDMS stamp, i'm new to NIL.

Thanks,
Andrea

> Hi,
>  What kind of stamps u need, whether PDMS based stamps or hard stamps. you
> can find sylgard 184(dow corning sells this). It is a mixture to make PDMS
> stamps for your desired pattern needs. I am not completely sure if any
> company is making stamps as you need. But you can get information on
> comapnies and research centers that are working with NIL...
>
> follow this link : http://www.napanil.org/
>
> Righeira
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review