MEMSnet Home: MEMS-Talk: SU8_2005 tailing at foot
SU8_2005 tailing at foot
2011-11-17
Xiaohui Lin
2011-11-19
gau s
2011-11-20
Gong Li
SU8_2005 tailing at foot
Xiaohui Lin
2011-11-17
https://lh6.googleusercontent.com/-svOBwLQuAXk/TsRyKCq3HqI/AAAAAAAAACM/Y07BUFTq6
ok/s912/SU8_2005_1114_onSi_10s09.jpg

Hi :   I am processing SU8 2005 on Silicon. But the shape is not what I
expected. There are tailing towards the trench at the foot the SU8, as the
picture shown in the link above. Could anyone suggest what I can do to
eliminate the tailing?

Thanks
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.