PZT in KOH
Amod Hulge
2011-11-19
Hi

You can try to using apeizon wax - grade W. This softens at 85
degree Celsius. You may need to come down a bit with KOH bath temp.
http://www.sisweb.com/vacuum/sis/apzwaxes.htm I have came across a paper,
where they have used this successfully. It is also possible to use LPCVD
silicon nitride thin layer. You can think of using fixtures from AMMT -
http://www.ammt.com/content/products.html

Hope this helps you.

amod
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.