MEMSnet Home: MEMS-Talk: Long DRIE O2 cleans?
Long DRIE O2 cleans?
2011-11-29
Michael Martin
2011-11-30
ashwini jambhalikar
Long DRIE O2 cleans?
Michael Martin
2011-11-29
Hi guys,

   We have a user that has been doing some carbon nanotube oxygen etching
using the ICP source on our STS DRIE.  He claims that in order to get his
process to work well (to completely stop silicon etching) he has to O2
clean the chamber for up to 2 hours (I'm guessing 600W of ICP).  I have
concerns that our O-ring for the Helium cooling chuck will be damaged in no
time as I seem to recall the STS suggests only 15 minutes of O2 clean.  I
will contact STS as well but wanted do get some opinions from this forum as
well.

Thanks,
  Michael
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.