MEMSnet Home: MEMS-Talk: silver plating on Pd2Si
silver plating on Pd2Si
2011-12-06
Rob MacDonald (rmacdonald)
silver plating on Pd2Si
Rob MacDonald (rmacdonald)
2011-12-06
I'm trying to plate silver on palladium silicide. If I don't activate the
palladium silicide with some sort of etch then there is very poor adhesion of
the silver to the silicide.

I have found that HF works, but the HF is very aggressive at attacking the
silicide itself. In particular it causes the silicide layer to peel. I found
some papers that show that HF will electrochemically etch silicon in the
presence of Pd. I suspect that this is the cause.

Wondering if anyone has had this problem and could suggest another chemistry to
activate the silicide surface prior to plating.

Thanks,

Rob MacDonald


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing