MEMSnet Home: MEMS-Talk: Soldering problem on gold metallization pads
Soldering problem on gold metallization pads
2012-02-15
Kabla Meni
Soldering problem on gold metallization pads
Kabla Meni
2012-02-15
Hi All,

I'm trying to solder AuSn bumps on Cr/500nm Au metallization, which is directly
on silicon. For some reason, the wettability of the solder to the pad is very
poor. It looks like there is some passivation layer on the surface of the
metallization pad.

The wafers with the Cr/Au metallization pass the following steps before
soldering:

1. Metallization (lift off, EB evaporation)
2. DRIE device and Handle
3. PECVD of silicon oxide on the metallization side
4. BOX and PECVD oxide etch by BHF
5. Wafer clean: EKC, Pirhana, SC-1

Does anyone have any ideas about what can cause the soldering problem?

Regards,
Meni

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation