MEMSnet Home: MEMS-Talk: week adhesion of SU8 to glass or quartz
week adhesion of SU8 to glass or quartz
2012-03-06
Xiaohui Lin
2012-03-07
Kipp Schoenwald
2012-03-07
Xiaohui Lin
week adhesion of SU8 to glass or quartz
Xiaohui Lin
2012-03-06
hi all:

    Could any one suggest how to improve the adhesion of SU8 2005 to glass
or quartz?

     I tried glass+omnicoat+SU8, it is week. I also tried
quartz+omnicoat+SU8 , but still peel off when I put in plating solution
(pH=5).

    Will HMDS work? or other adhesion promoter?

thanks
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.