2012-03-09
Lina Gonzalez
2012-03-12
Michael Martin
2012-03-23
David Roberts
2012-03-23
Maria Matschuk
2012-03-23
Kevin Nichols
Intermediate layer of tantalum
David Roberts
2012-03-23
Hi Lina,
My thin film head experience is - Sputtered (PVD) deposited NiFe will stick
pretty well to oxides like glass or Alumina. NiFe/alumina is used in
production. Refractory metals will stick the best to oxides and coinage
metals the worst.

This is it -
Metals like Al, Ti, Cr, Ta having a high affinity for oxygen will stick well
to oxides like glass. Gold, copper or platinum with a low affinity for
oxygen require an adhesion layer like TiW or Ta.

I hope this helps,
Dave

David Roberts (Wafer Plating Specialist)
Prodigy Surface Tech (408) 469-3203 cell
807 Aldo Ave., Suite 103
Santa Clara, CA 95054
Phone (408) 492-9390
FAX (408) 492-9391


-----Original Message-----
From: Lina Gonzalez [mailto:[email protected]]
Sent: Friday, March 09, 2012 7:12 AM
To: [email protected]
Subject: [mems-talk] Intermediate layer of tantalum

Hi all,

What is the special interaction between sputtered tantalum on glass that
makes tantalum stick to glass? For example, why would you want a Ta layer
before depositing NiFe when having a glass substrate?

Thanks,

Lina




_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group