Hello,

I am trying to find a wet etchant for etching either Al or Cr without
etching a ZnO thin film on the same sample. I cannot let the ZnO film to be
affected in any way, hence I can't even consider solutions with some degree
of selectivity. For reasons I can't go into detail here, lift-off is not an
option. It appears that ZnO is etched in pretty much any of the acids and
bases commonly found in semiconductor processing. I'd greatly appreciate if
someone would share any insight.

Thank you,
Bhargav.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer