Yingtao Tian
2012-06-27
Bill Moffat
2012-06-28
Gareth Jenkins
2012-06-28
Yingtao Tian
2012-06-28
Bill Moffat
2012-07-02
Yingtao Tian
2012-07-02
WANG Yingnan
2012-07-03
Yingtao Tian
2012-07-05
Yingnan Wang
Ultrathick SU8 photoresist processing
Yingtao Tian
2012-06-27
Dear All,

I am trying to make very thick SU8 photoresist on silicon wafer, however, I
found that, even the resist was spun coated, the surface will not be flat. I
tried to put over 200 um thick resist but the thickness can vary between 180 -
220 across the whole wafer. I have tried to adjust the levelness of the hotplate
by using an inclinometer and it was almost perfectly levelled. Somebody
suggested that the air turbulence in the cleanroom does matter for such very
thick resist. But, I have no evidence to doubt it.

Anybody has ideas?

Thanks,
Yingtao
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
The Branford Group
Mentor Graphics Corporation