MEMSnet Home: MEMS-Talk: Removal of crosslinked SU8
Removal of crosslinked SU8
2012-07-17
Yingtao Tian
2012-07-17
Karim Ogando
2012-07-17
Yingtao Tian
2012-07-17
Mike Whitson
2012-07-17
Shay
2012-07-17
Ad Hall
2012-07-17
Lukasz Urbanski
2012-07-20
Matthieu Nannini, Dr.
Removal of crosslinked SU8
Matthieu Nannini, Dr.
2012-07-20
Beware of O2 plasma, it will etch the chrome on your mask.
I would try 350°C (or more) bake for as long as you can. It might burn the SU8
away.

Matthieu

-----Original Message-----
From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of Karim Ogando
Sent: 17 July 2012 15:44
To: General MEMS discussion
Subject: Re: [mems-talk] Removal of crosslinked SU8

Hi Yingtao,

Maybe you can use O2 Plasma, but it is going to damage the thin oxide film on
the top of the chrome.

which is the thickness of the crosslinked SU8?

Best regards,

Karim

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation
Harrick Plasma, Inc.