Mark West
dicing particle contamination
[email protected]
2012-07-25
you can try cleaning in megasonic or dicing with a tape on both sides. it is
sometime tricky to remove the top tape since you have to somwhow get hold of it
at a corner to start pulling.

----- Original Message -----
From: ProtoSi Info 
Date: Wednesday, July 25, 2012 0:08
Subject: [mems-talk] dicing particle contamination
To: [email protected]

> Hello
>
> We've been struggling with particles getting embedded in our delicate
> silicon comb structures during dicing. Our current process involves
> spraying on a 10um thick layer of photoresist over the entire
> wafer and
> then do a soft bake. After dicing we rinse the wafer to remove
> particlesbefore stripping off the resist. However we're still
> getting particles
> stuck in-between the comb fingers. We've attempted ultrasonic
> cleaning but
> that damages the combs.
>
> Any tips to remove or prevent particles would be greatly appreciated.
>
> Thank you
> Kevin Chang
> ProtoSi
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
‭‮
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.