MEMSnet Home: MEMS-Talk: Pinhole-free, NON-POROUS anodic alumina?
Pinhole-free, NON-POROUS anodic alumina?
2013-01-04
Ned Flanders
Pinhole-free, NON-POROUS anodic alumina?
Ned Flanders
2013-01-04
Hey all,


apparently, it is possible to anodize aluminum to obtain non-porous
(pinhole-free) alumina. What's the trick, and how thick could the
layer be, at most?


Thanks in advance


m
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.