MEMSnet Home: MEMS-Talk: High contrast photoresist for interference lithography
High contrast photoresist for interference lithography
2013-01-15
Justin Hannigan
2013-01-15
Daniel Figura
2013-01-16
Justin Hannigan
2013-01-16
Andrew Sarangan
2013-01-16
Justin Hannigan
High contrast photoresist for interference lithography
Justin Hannigan
2013-01-16
On 1/15/2013 1:03 PM, Daniel Figura wrote:
> High resolution is relative - what L/S resolution do you need? Limiting
> factor can be photo resist contrast but very often exposure system.
I'm trying to print dense lines with a period of 3000 l/mm currently.
So, approximately 170 nm linewidth.  I have gotten good results with SPR
220, as I mentioned.  But this was with a different exposure setup.  I
will verify that we can obtain similar results with the current setup.

> Some time ago I made a list of commercially available UV photo resists
> http://www.smartfabgroup.com/photoresists.php  have a look.
Thank you.  I found your list some time ago and have found it very
useful to get an overview of various resists.

Justin

--
Justin M. Hannigan, Ph.D.
Process Development Engineer
LightSmyth Technologies,Inc.
875 Wilson St, Unit C
Eugene, OR 97402
Tel: 541-431-0026
www.lightsmyth.com


!DSPAM:50f6dee2205381192612421!


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation