MEMSnet Home: MEMS-Talk: Polyimide / glass adhesion failure
Polyimide / glass adhesion failure
2012-11-19
Sheng Zhang
2013-01-19
Yunda Wang
2013-01-21
Michael Martin
2012-11-20
[email protected]
Polyimide / glass adhesion failure
Yunda Wang
2013-01-19
Did you use adhesive promoter?For example, VM-652?

2012/11/19 Sheng Zhang 

> brine





--
Yunda Wang, Ph.D.
Department of Mechanical engineering
University of Colorado - Boulder
Boulder,Co. US. 80302
(614)3120920
E-mail: [email protected]
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering