MEMSnet Home: MEMS-Talk: RIE etch Si3N4 over InAs
RIE etch Si3N4 over InAs
2013-03-01
S M Shazzad Sharif Rassel
RIE etch Si3N4 over InAs
S M Shazzad Sharif Rassel
2013-03-01
Hi all,

I am planning to RIE etch Si3N4 over InAs
using  SF6 and O2.

Does anyone have any experience about the selectivity of
nitride over InAs?

Regards,
S M Shazzad Sharif Rassel
University of Oklahoma
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics