work with thin wafers
Tang Tian
2013-05-23
Good afternoon Hong,

Could you elaborate more on your process?

Which type of bonding technique you are using?

How does the substrate break, e.g. mechanical, thermal, or else?

We, EV Group, have extensive experience on wafer bonding, thin wafer handling,
and temporary bonding followed with debonding.   We will be happy to help at our
applications lab in Tempe, Arizona.


Best Regards,
Tian Tang

EV Group
invent * innovate * implement
Applications Engineer - Direct: +1 (480) 305 2455, Main: +1 (480) 305 2400 Fax:
+1 (480) 305 2401
Cell: +1 (480) 274 3892
E-Mail: [email protected]
Web: www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.
Save paper and trees! Please consider the environment before printing this
e-mail.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.