MEMSnet Home: MEMS-Talk: Alternative route for amine deposition on glass
Alternative route for amine deposition on glass
2013-06-19
jagannath s
2013-06-20
André Bödecker
Alternative route for amine deposition on glass
jagannath s
2013-06-19
I am trying to functionalize glass surface with amine groups to immobilize
proteins. I also need to incubate this surface with a strong acid
(Trifluoroacetic acid) for upto 20 minutes.
I have tried types and deposition of amino-silanes like aminopropylethoxy
silanes, dipodal silanes etc, but fear the layer is not stable to the acid.
Does anyone know about alternative methods/chemicals for amine
functionalization?
Any thoughts or comments is greatly appreciated

Thanks
Jagannath
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing