MEMSnet Home: MEMS-Talk: LOR 3A and Borosilicate
LOR 3A and Borosilicate
2013-08-26
Martin,Michael David
2013-08-26
Lou Chomas
LOR 3A and Borosilicate
Martin,Michael David
2013-08-26
Hi,
  Does anyone have experience with LOR3A (w/ 1827) on borosilicate glass.  The
processing parameters, i.e. undercut rate after a 6 min 150C bake, appear quite
different than those for silicon.  That is, I am seeing a much lower undercut
rate for the borosilicate than for silicon.

Thank you,
  Michael
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering
Harrick Plasma, Inc.