A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Specularity of Gold
Specularity of Gold
1999-07-01
Vamsee K. Pamula
Specularity of Gold
Vamsee K. Pamula
1999-07-01
Hello All,

Does anybody know the temperature at which a thin film (0.5 um) of Gold
looses its specular property.

In particular, I would like to know the temperature beyond which Gold
looses its good reflectance and becomes rough, for a MUMPS fabricated Gold
on Polysilicon2 layer with a thin Chromium adhesion layer in between.


Thanks,
Vamsee Krishna
Dept of Elec Engg'
Duke University
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Nano-Master, Inc.