2013-12-06
Elhadi hadi
2013-12-06
[email protected]
MEMS Fabrication
Elhadi hadi
2013-12-06
Dear Colleague,

I am new in that field and I need help in the following cases


*Case A:*

Metal layer (not specific layer) is deposited on a Silicon wafer. After
that, we add a layer of photoresist and this layer has particles in
different levels. We put the device in Mask aligner using mask to expose UV
light.



*Case B*

Same as case A but there is no metal layer between the Silicon wafer and
the photo resist.


*How can I indicate the resultant morphologies of the Photoresist pattern
on wafer each case?*

Thank you,
Regards

Hadi
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.