this is CMOS related and not MEMS.in CMOS when you use LOCOS isolation, you
sometime implant below the pad ox (the oxide below the nitride) in order to
prevent leakage between the channels that can happen due to inversion layer
foramtion.a guard ring is a implanted ring around the channel to prevent latch
up of naturally occurring NPN or PNP parasitic transistors in a CMOS circuit.

Shay

 ----- Original Message -----From: bhargav panchal
Date: Thursday, March 13, 2014 16:27Subject: [mems-
talk] DifferenceTo: "[email protected]" > Hi> > Hello
My name is Bhargav. I am vlsi student.I am confused in the > difference between
channel stop-implant and guard rings. Their > purpose and fabrication are
same....> > I searched over internet but no answer. Please if you have > answer
let me know....> > Thank you> Bhargav>
_______________________________________________> Hosted by the MEMS and
Nanotechnology Exchange, the country's leading> provider of MEMS and
Nanotechnology design and fabrication services.> Visit us at http://www.mems-
exchange.org> > Want to advertise to this community?  See
http://www.memsnet.org> > To unsubscribe:> http://mail.mems-
exchange.org/mailman/listinfo/mems-talk‭‮
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing