su-8 2002 removal method
Tong CHEN
2014-04-04
On 4/3/14 7:54 PM, shay kaplan wrote:
> SU8 is an epoxy and you need an epoxy stripper to take it off.
> If I remember right, Microchem sells a material that you spin under the SU8
that enables you to remove it later
>
> -----Original Message-----
> From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of ???
> Sent: Thursday, April 03, 2014 8:28 AM
> To: General MEMS discussion
> Subject: [mems-talk] su-8 2002 removal method
>
> I used SU-8 2002 for sacrificial layer(about 2um).
>
> after whole process is finished, I want to remove SU-8 layer.
>
> but, it is very hard. I used Remover PG(80℃, 30min) but it is
indissolubleness(?).
>
> For forming mems sensor, the metal layers are deposited around a SU-8 layer.
>
> So I want to remove SU-8 2002 without damages of other structures.
>
> How can I do it?
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hello,

you can try Omnicoat. That sacrificial layer will help remove the SU8.

--
Tong Chen
Postdoc
SyntheCell Team
IGDR CNRS UMR 6290
2, Avenue du Professeur Léon Bernard
35043 Rennes
France

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
University Wafer
MEMS Technology Review