Hello,

I'm trying to find a way to etch aluminum oxide without attacking titanium.
Several common Al2O3 etchant I tried all etch Ti quite fast as well, such
as NaOH, H3PO4, NH4OH, etc. Can anyone suggest a way to achieve selective
etching between these two?

Any advice will be greatly appreciated! Thank you very much!

--
Travis
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer