Removal of silane coating
Bill Moffat
2014-09-29
Any organic eater, Oxygen plasma, peroxide and sulphuric acid. How thick is the
silane and what specific silane? Bill Moffat

Sent from my iPad

> On Sep 29, 2014, at 7:20 AM, "JJ HU"  wrote:
>
> Hi all,I am wondering if there is way to remove silane/silanization coating
from PDMS or glass?
> Thank you in advance!
> JJ Hu
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing