Hi All,

I'm looking for a way to treat SU-8 to keep either a dilute or solventless
PDMS off of certain areas. I'm not sure there is much of an option out
there, but I'm looking for something specific that can offer this property.

Ideally, I'd like to do normal SU-8 processing up through PEB, coat the top
of my SU-8 with this silicone-phobic material, develop away the unexposed
SU-8, and coat with PDMS to end up with it only in the trenches I defined
by photolith. Just curious if there is anything out there, sort of a
corollary to silanization of glass for water repellency.

Thanks,
Dave
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer