MEMSnet Home: MEMS-Talk: Shrinkage problem on SU8 layer on Si Substrate
Shrinkage problem on SU8 layer on Si Substrate
2014-10-23
KarthiKeyan K
2014-10-23
Andrew Sarangan
2014-10-27
KarthiKeyan K
2014-10-27
Bill Moffat
2014-10-28
Sajeesh P
2014-10-29
Andrew Sarangan
2014-10-27
Sajeesh P
Shrinkage problem on SU8 layer on Si Substrate
Andrew Sarangan
2014-10-23
Can you elaborate how you are determining this shrinkage? During softbake
there will be loss of solvents and a change in thickness, but it should not
cause any stresses because the uncured SU8 should reflow above 65C. Perhaps
your ramp rate is too fast causing part of the SU8 to flow while other
parts are still solid?

On Wed, Oct 22, 2014 at 10:49 PM, KarthiKeyan K 
wrote:

> Dear All,
>
> I am facing shrinkage problem on SU8 2075 photoresist layer on Silicon
> Substrate. Actually this problem accruing on soft backing process at 65C on
> hotplate & hot air oven also.
>
> Kindly suggest to over come this problem.
>
> Thanking you,
>
> Best Regards,
> Karthi
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing