MEMSnet Home: MEMS-Talk: PDMS bonding to silicon for micro-channel heat sinks
PDMS bonding to silicon for micro-channel heat sinks
2015-06-09
Leily Majidi
2015-06-10
André Bödecker
2015-06-11
Nathan McCorkle
2015-06-15
André Bödecker
2015-06-16
Bill Moffat
PDMS bonding to silicon for micro-channel heat sinks
Nathan McCorkle
2015-06-11
On Tue, Jun 9, 2015 at 10:37 PM, André Bödecker
 wrote:
> Hello Leily,
>
> anodic bonding is an expensive, but very reliable process. Structuring of
> glass wafers is not a big problem. You can contact me if you are interested.
>
> Bonding with PDMS normally needs only an oxygen plasma activation of the
> surfaces. There are also some special adhesion promoters if necessary. But a
> tight bonding will only work if the PDMS has a good uniformity and that will
> be a difficulty over a whole 100 mm wafer, I assume. We use the Sylgard 184
> 2k-silicone ("PDMS"; Dow Corning). Even spin-coating leads to an edge bead
> which inhibits a complete contact between two wafers.

How do you get around this? Do you adjust the spin-coating or
viscosity of the resin? Or do you simply cut/dice the bead area away?
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing