Ali Alsaqqa
2015-10-15
André Bödecker
2015-10-16
Andrew Sarangan
2015-10-19
Ali Alsaqqa
2015-10-20
Andrew Sarangan
2015-10-26
Ali Alsaqqa
2015-10-19
[email protected]
Best way to make elemental Cr films
Andrew Sarangan
2015-10-16
The 10^-7 Torr during evaporation is a pretty decent vacuum level, and the
oxidation rate should be very minimal especially if you keep the deposition
rate high.



On Mon, Oct 12, 2015 at 8:44 PM, Ali Alsaqqa  wrote:

> Hello all,
>
> I would like to know what is the best way to prepare films of elemental
> Chromium. Exact thickness does not matter, but something like hundreds of
> nanometers should be fine. The target measurement is simple transport (I,
> V) in the presence of some magnetic field.
>
> My main concern here is oxidization. I was thinking about depositing the
> films using e-beam evaporator, but it can attain a vacuum of only 10-7
> Torr, and with this level oxidization will occur. MBE is not an option at
> the moment.
>
> I was also thinking about buying wafers from commercial sectors, but I will
> run into the same problem, i.e. the surface will oxidize as soon as it
> contacts air.
>
> Are there any suggestions?
>
> Ali M. Alsaqqa,
> PhD candidate,
> Department of Physics,
> University at Buffalo, NY, USA
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review
Addison Engineering