A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicon Carbide Issue
Silicon Carbide Issue
2015-12-08
bhargav panchal
2015-12-09
Morrison, Richard H., Jr.
2015-12-09
André Bödecker
2015-12-10
Kumar, Parshant
Silicon Carbide Issue
bhargav panchal
2015-12-08
We have problem regarding nickle deposition on Silicon nitride by sputtering.
Prior to deposition we have removed the oxides from the surface. Please suggest
possible solution.

Have a good day everyone.

Regards, Bhargav Panchal+91 9742712671
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer