MEMSnet Home: MEMS-Talk: Eutectic Au bonding
Eutectic Au bonding
1999-07-13
Tang fei
Eutectic Au bonding
Tang fei
1999-07-13
Hello,

We want to use eutectic Au bonding technology. Can anybody tell me what
thickness of the Au film is proper? What condiction ,such as temperature and
pressure, is needed for this kind of bonding? And whether the eutectic Au
film after bonding can be used as conductor?
Thank you very much for your information.

Best regards,

F. Tang