MEMSnet Home: MEMS-Talk: strange phenomenon during O2 ashing of PR
strange phenomenon during O2 ashing of PR
2016-02-04
Andrew Xiang
2016-02-08
Andrew Sarangan
strange phenomenon during O2 ashing of PR
Andrew Xiang
2016-02-04
When I was ashing S1800 photoresist using Pure O2, I noticed the following:
After 5 min, or 7min, the photoresist layer stayed the same. The layer is
only 0.5um thick to begin with.
But if I look at it after 10min, all PR is gone.  Seems it is hard to find
the middle point.
Does the O2 plasma turn everything in ash first and then poof, everything
is gone? I thought it
etch layer by layer.

Power is pretty low, 200W, 0.1-0.2torr. Pure O2, RF plasma.

-Andy
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer