MEMSnet Home: MEMS-Talk: RE>Youngs Modulus and Poisson ratio of Parylene C
RE>Youngs Modulus and Poisson ratio of Parylene C
1999-07-16
Dan Brewer
RE>Youngs Modulus and Poisson ratio of Parylene C
Dan Brewer
1999-07-16
         RE>Youngs Modulus and Poisson ratio of Parylene C
Youngs Modulus of Paralene C is 400,000 psi. I'm not quite sure what your
looking for when you ask about Poisson ratio.

Dan Brewer
Technology Analyst
Brewer Science, Inc.

--------------------------------------
Date: 7/15/99 8:50 PM
To: Dan Brewer
From: Cheol-Hyun Han
Hello,

Does anyone has info. about Young's Modulus and Poisson ratio of Parylene C ?
Any any info. will be highly appreciated.

Thanks!


RFC-822 Header:


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.