MEMSnet Home: MEMS-Talk: e-beam evaporation of SiO2
e-beam evaporation of SiO2
2018-06-07
Mehmet Yilmaz
2018-06-14
Brad Cantos
e-beam evaporation of SiO2
Mehmet Yilmaz
2018-06-07
Dear mems-talk community,
We are interested in e-beam evaporation of thick layers (from 6 microns up
to 16 microns) of SiO2.
We wonder if anybody from the mems-talk community have any experience with
such thick layers of SiO2 e-beam evaporation in terms of mechanical
properties such as Young's modulus and residual stress?

Based on the feedback from the mems-talk community we may decide to proceed
directly with our actual work, or do some preliminary experiments before we
start our actual work.

Sincerely,

Mehmet
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.