Iwan Sukirna
coating cd,zn,polymer etchants
Iwan Sukirna
1999-10-20
hello

i have problem with my samples for my research in final project
my problem is etchant for coating by Cd, Zn, and some kind polymer/paint
coating.

tthe goal is:define the  phase, process (hot dip or e-plating)
and to differ in the boundary with base metal (steel)

therr refference about polymer is some kind 'PTFE'
but i'm not sure it is.

please for contact person mailto [email protected]
becaus the other one under construction...

materials sci & eng
bandung inst. of tech
koordasmet

***********
iwansukirna
***********
[email protected]
[email protected]
022-2042487


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing