Drilling in Acrylic
1999-11-22
Penney Robert
Drilling in Acrylic
Penney Robert
1999-11-22
This message is in MIME format. Since your mail reader does not understand
this format, some or all of this message may not be legible.

------_=_NextPart_001_01BF3517.96B018CA
Content-Type: text/plain;
        charset="iso-8859-1"


I am experiencing difficulties in drilling a 0.3mm (.02") diameter hole in a
3mm (1/8") thick piece of acrylic.  The problems are associated with
material removal and melting.

I am using a Bridgeport with a drill bit and have experimented with spindle
speed and feed rate, but haven't acheived an optimal hole.

Any information on a good guide for machining plastic or any personal
experience on drilling plastic would be appreciated.

Thanks!!

Penn

Orchid Biocomputer
303 College Rd E
Princeton, NJ  08540

609-750-2268

------_=_NextPart_001_01BF3517.96B018CA
Content-Type: text/html;
        charset="iso-8859-1"




GreenBoy Stationery



 
I am experiencing difficulties in drilling a 0.3mm (.02") diameter hole in a 3mm (1/8") thick piece of acrylic.  The problems are associated with material removal and melting.
 
I am using a Bridgeport with a drill bit and have experimented with spindle speed and feed rate, but haven't acheived an optimal hole.
 
Any information on a good guide for machining plastic or any personal experience on drilling plastic would be appreciated.
 
Thanks!!
 
Penn 
 
Orchid Biocomputer
303 College Rd E
Princeton, NJ  08540
 
609-750-2268
------_=_NextPart_001_01BF3517.96B018CA--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer