Deposit nitride on 3" wafer
.
1999-11-30
This is a multi-part message in MIME format.

------=_NextPart_000_0005_01BF3B43.9A030500
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable

I am looking for a company that can deposit nitride on 3" wafers.

Any ideas?

Tom Kern
CESCO
Arizona, USA
[email protected]


------=_NextPart_000_0005_01BF3B43.9A030500
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable








I am looking for a company = that can=20 deposit nitride on 3" wafers.
 
Any ideas?
 
Tom Kern
CESCO
Arizona, USA
[email protected]
 
------=_NextPart_000_0005_01BF3B43.9A030500--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.