> about the potential danger of contamination from Platinum and we could use

Like Au, Pt is used to adjust carrier lifetimes in high voltage
transistors. It introduces donor and acceptor deep levels which are
effective generation-recombination centers.  In other words, it is a
lifetime killer and should be used with extreme caution.

- r.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation