MEMSnet Home: MEMS-Talk: Re: looking for adhesive
Re: looking for adhesive
1999-02-02
Shekhar Bhansali
1999-02-02
Alexander Shenderov
Re: looking for adhesive
Alexander Shenderov
1999-02-02
make it.  Plenty of recipes around, I recommend (w/w/w) 110 kaolin/480
sodium silicate/410 graphite powder.  Mix real good!!! use within 3
hours.  Bake for 45-60 minutes at 160C.  It's good to 350C, chemically
resistant and conductive as a side bonus.

Make sure your powders are fine enough for your dimensions!

Good luck

Alex


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing