Re: Better resolution for desktop publishing masks
1999-02-05
Ashutosh Shastry
1999-02-05
Mark Bachman
1999-02-05
Ji Fang
1999-02-05
Ashutosh Shastry
1999-02-09
Ashutosh Shastry
1999-02-05
[email protected]
1999-02-08
Amit Shiwalkar
Re: Better resolution for desktop publishing masks
Ashutosh Shastry
1999-02-09
Hello,

        There have been quite a few queries about my prevous mail so I
thought of mailing some details to the group.

1. It is SciTek 3130.  There could be other high resolution printers which
are routinely used by Offset printers in Bombay who cater to ad ajencies
to provide images in print.

2. Bromides is an option.  You can decide positive or negative while
firing.  The postscript file can be used to get either output.

3. If you specify SCREEN PRINTING then emulsion is down.
   If you specify OFFSET PRINTING then emulsion is up.

4. The film is TRANSPARENT to uv and the printed lines are NOT. We've
directly used it for lithography and got good results.

Hope this info is useful.

Regards,

-Ashutosh-



On Mon, 8 Feb 1999, George Raicevich wrote:

>
> Dear Ashutosh
>
> I was very interested in what you had to say regarding the Infra Red (IR)
> printer.
>
> I would like to try an find one locally to try out for making some chrome
> on quarzt masks for an excimer laser.  Do you have any more details on the
> brand or type of printer , what the output consists of (bromides ?) whether
> you can specify positive or negative , whether the image can be placed on
> the under side or the top side of the film.  Also I want to use the image
> for a contact print 1:1 on the quartz mask that requires UV light. I wonder
> if the film used on the IR print is transparent to UV ?
>
> I would be grateful for any advice, and can summarize  the results for the
> MEMS net . Thanks

================================================================================
        Ashutosh Shastry                Graduate Student,
        #30, Vihar House, IIT,          School of Biomedical Engineering,
        Powai, MUMBAI-76.               I.I.T. Bombay.

        Microlelectronics Staff Room,  Phone/Fax: 578 3655 or 5782545 extn 8471
        EE Dept., I.I.T. BOMBAY.        Fax: 579 3707

===============================================================================
        Dream as if you will live forever
                                          Live as if you will die today.
================================================================================


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Addison Engineering
Mentor Graphics Corporation