Have you investigated the usage of an FIB (Focused Ion Beam) system
instead??
Best regards,

Steve Rosenberg
Deschutes Corporation
17400 SW Upper Boones Ferry Rd #240
Durham OR 97224
(503) 443-3602 Fax: (503) 443-2353 Mobile: (503) 312-4647
Email: [email protected]
-----Original Message-----
From: Thomas Ammer 
To: [email protected] 
Date: Friday, February 05, 1999 12:34 PM
Subject: direct lasert writing in thick resist


>Dear Colleagues,
>
>I am trying to fabricate 3D structures in thick positive photo resist
>(20-50 micron) by direct laser writing with a blue laser (440nm).
>Does anybody have experience, which type of resist is best suitable for
>this purpose?
>At the moment I am using Microposit S1828. It has good properties for
>thin films, but exceeding 10 micron, the softbake procedure seems to be
>too critical.
>The very surface layer is almost development-inhibiting, which results
>in a very inhomogenous development for shallow structures.
>Unfortunately, most thick film resist are optimized for high contrast
>and aspect ratios, which is disadvantegous if you want to obtain
>arbitrary depths.
>
>Thank you and with best regards, Thomas Ammer.
>
>
>Thomas Ammer
>CSEM  Micro-Optics
>Badener Str. 569
>8048 Zurich
>Switzerland
>Tel: +41 1497 1434
>[email protected]
>
>
>
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
Mentor Graphics Corporation