Boron Etch Stop
Kavita Chandra
1999-02-24
======== Original Message ========

--------------DF62BCAFF0AB640A39C87D3C
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

I am using a boron etch stop to build a hinge on silicon. What is the
best anisotropic etchant to use. I am considering KOH, TMAH, EDP, etc.

--
Steve Forgrieve
Department of Electrical Engineering
The University of Edinburgh
King's Buildings
Mayfield Rd
Edinburgh EH9 3JL
(Int +44) 131 650 5665 (enquiries)
email: [email protected]



--------------DF62BCAFF0AB640A39C87D3C
Content-Type: text/html; charset=us-ascii
Content-Transfer-Encoding: 7bit



I am using a boron etch stop to build a hinge on silicon. What is the best
anisotropic etchant to use. I am considering KOH, TMAH, EDP, etc.
-- 
Steve Forgrieve
Department of Electrical Engineering
The University of Edinburgh
King's Buildings
Mayfield Rd
Edinburgh EH9 3JL
(Int +44) 131 650 5665 (enquiries)
email: [email protected]
  --------------DF62BCAFF0AB640A39C87D3C-- ======== Fwd by: Kavita Chandr ======== I have used KOH very successfully with Boron Etch Stop. Works very well. Kavita Chandra MEMS Design Engineer Wilcoxon Research Inc. (301)216-3032 -voice (301) 330-0743 -Fax
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review