A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Thick Resists for Au plating
Re: Thick Resists for Au plating
1999-02-10
Shekhar Bhansali
1999-02-10
Keith Jackson
1999-03-01
Mark Wendman
Re: Thick Resists for Au plating
Mark Wendman
1999-03-01
If I am not mistaken SU-8 is removable in epoxy resin strippers. I do not
know
more specifics.

Mark Wendman
[email protected]

----------
> From: Todd Green 
> To: [email protected]
> Subject: Thick Resists for Au plating
> Date: Tuesday, February 09, 1999 10:35 AM
>
> Hi,
>
> I'm looking for resists that can be spun up to around 25 microns and have
> good compatability with alkaline (pH=10) gold sulfite plating bath. We
are
> using SJR 3740 but are interested in other alternatives. We tried SU-8
> but can't find anything to remove it. Is there anything else available?
>
> Thanks,
>
> Todd Green
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group