MEMSnet Home: MEMS-Talk: looking for cleaning solution
looking for cleaning solution
1999-03-05
lsjang
looking for cleaning solution
lsjang
1999-03-05
This is a multi-part message in MIME format.

------=_NextPart_000_001A_022E83EE.5F48AEC0
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable

Hi,

I am working on micropump now. The pump was made by silicon and pyrex =
and bonded on alumium base by crystal bond. Since the inside of the pump =
got dirty, I am looking for a kind of cleaning solution to remove =
organic and dust from the surface of silicon and pyrex, but not to =
dissolve crystal bond, pyrex and metal. Could you give me some opinions? =
Thanks a lot!
=20
Ling-Sheng

------=_NextPart_000_001A_022E83EE.5F48AEC0
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable









Hi,
 
I am working on micropump now. The=20 pump was made by silicon and pyrex and bonded on alumium base by crystal = bond.=20 Since the inside of the pump got dirty, I am looking for a kind of = cleaning=20 solution to remove organic and dust from the surface of silicon and = pyrex, but=20 not to dissolve crystal bond, pyrex and metal. Could you give me some = opinions?=20 Thanks a lot!
 
Ling-Sheng
------=_NextPart_000_001A_022E83EE.5F48AEC0--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.