Re: Glass Etch
Yit-shun Leung Ki
1999-03-03
Hi,

I've never heard of anisotropic etching of glass although perhaps some
kind of dry etching would be possible. To the rest of the MEMS group,
I'd be very interested in the answer also!

Cheers.
--
Yit-shun Leung Ki
Graduate Student in Microfluidics
_______________________________________________________________
Institute of Microsystems (IMS)
Dept. of Microengineering,
Batîment BM,
Swiss Federal Inst. of Tech. (EPFL),    TEL: +41 21 693 7818
CH-1015 Lausanne                        FAX: +41 21 693 5950
Switzerland                             URL: dmtwww.epfl.ch/ims


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.