Does anybody know which gas is suitable for dry etching platinum ?

Thanks

Emmanuel Dubois

 ___________________________________________________________________
          __  ____  __       __  __  __
       / /_/ / / / / /  _ / /_  /_/ / /
      / /_  / / / / /    / __/ /_  / /

     Institut d'Electronique et de
     Microelectronique du Nord
     UMR CNRS 8520
     Departement ISEN
     Avenue Poincare B.P.69
     59652 VILLENEUVE D'ASCQ  CEDEX
     tel: (+33) 3 20 19 79 16
     fax: (+33) 3 20 19 78 84
     e-mail:[email protected]
     http://www.isen.fr/isen-lci/quest

___________________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing